Determine the compression ratio first, then determine the groove depth
Whether the sealing ring can stop water for a long time depends on how much it is compressed, not how tightly it is pressed. For common silicone or nitrile O-rings, the design compression rate is 20%-30%, which is relatively safe: insufficient compression, the microscopic unevenness of the sealing surface will not be filled; excessive compression, the stress relaxation of the rubber material will be accelerated, and water will start to leak after half a year due to insufficient rebound.
The groove depth is back calculated from the wire diameter and compression rate. Taking an apron with a wire diameter of 2.0 mm as an example, 25% compression corresponds to a groove depth of 1.5 mm, and the groove width is 1.25–1.35 times the wire diameter to leave room for lateral expansion of the rubber material. If the groove width is narrowed, the rubber will have nowhere to go, which will push up the upper cover and damage the fit. The bottom of the groove should not be made with sharp corners. A rectangular groove with small rounded corners is more conducive to the flow of rubber, and the mold processing and cleaning are convenient.
Flange stiffness and screw spacing
Many water intrusion cases are not caused by the rubber ring, but the cover plate is bent by the water pressure and the reaction force of the rubber ring between the screws. The greater the distance between the two screws, the greater the gap in the middle. From experience, the M3 screw spacing is controlled within 45 mm, and the M4 screw spacing can be relaxed to about 60 mm. At the same time, the flange edge should be thickened or reinforced on the inside. If studs or buckles are arranged near the sealing surface, space must also be made for the rubber ring to prevent the part from being squeezed to the point of no return.
The flatness of die castings is also critical. If the plane where the sealing groove is located is warped as a whole, the compression amount of the rubber ring will be unevenly distributed along the circumference, and the thin side will fail first. Weijiaxin left a margin on the sealing surface and then fine-milled it, and marked the flatness requirements on the drawings during the review as a common acceptance item for die-casting and machining.
How to do structural verification
The verification method must be determined during the drawing review stage. It is more convenient to perform an air tightness test after the whole machine is assembled than to directly immerse it in water: fill the casing with 20-30 kPa air pressure, hold the pressure for 60 seconds and observe the pressure decay; when conditions permit, use the pressure difference method to determine whether the leakage point lies in the sealing ring, outlet hole or lens window. Before testing, it is necessary to confirm that there are no shrinkage holes in the die-cast shell itself. Local looseness will also show up as slow leakage and can easily be misjudged as a rubber ring problem.
- The groove depth is measured point by point with a depth micrometer, with no less than 8 points along the circumference;
- The assembly torque is given according to the screw specifications and randomly checked, and tightening is not based on the feel;
- The rubber ring is thinly coated with silicone grease before assembly to reduce distortion and undercut;
- The first batch of prototypes are retested for air tightness after high and low temperature cycles to verify rebound.
Sealing is a system problem and cannot be solved by thickening the rubber ring alone. Once the compression ratio, flange stiffness and flatness are determined, it makes sense to talk about the waterproof level.