Seal groove size and compression calculation

Why compression is the core parameter

Whether the seal can be effective for a long time depends largely on how much the rubber ring is compressed. If the compression rate is too low, the contact stress is insufficient, and water vapor penetrates under capillary action; if the compression rate is too high, the rubber will be in a high stress state for a long time, and the compression permanent deformation will be accelerated, and it will lose its rebound after several disassembly and assembly. The empirical range is 20 to 30 percent of the cross-sectional diameter. The upper limit is used for static flat seals and the upper limit is used for parts that require repeated disassembly and assembly.

How to calculate the groove size

Take commonly used circular cross-section sealing rings as an example. The groove depth is equal to the cross-sectional diameter minus the design compression amount. The groove width should allow for the volume space after the rubber material is compressed. Generally, it is 1.1 to 1.3 times the cross-sectional diameter. When the filling rate exceeds 85%, the rubber has no place to go and will be extruded inward and push against the mating surface, forming a water seepage channel instead.

Calculations cannot only use nominal dimensions. There is a draft angle between the groove bottom and groove wall of the die-casting part, and the CNC-machined groove edge will leave a tool tip fillet, which will cause the actual compression amount to deviate from the drawing. It is recommended that the groove depth and the flatness of the groove bottom be marked on the drawing at the same time, and the flatness of the mating surface be constrained at the same time. Otherwise, if the two surfaces are each qualified, the gap may still be uneven when pressed together.

Frequently Asked Questions and Inspection Methods

Under typical working conditions, water seepage points often appear at the corners of slots and near screw holes. The rubber material is stretched at the corners and the cross-section becomes smaller; local warping occurs near the screw holes due to improper tightening sequence. The solution is to enlarge the corner fillet to the extent that the rubber ring can fit naturally, and specify on the process card to tighten it diagonally in stages.

  • Cross-section inspection: measure the cross-section diameter of the rubber ring in each batch and control it near the tolerance median
  • Groove depth measurement: use a depth micrometer to take five points evenly along the groove
  • Indentation inspection: observe whether the indentation width is after disassembly Continuous and uniform
  • Air tightness verification: the whole machine maintains pressure or is immersed in water, and records the pressure decay time

Weijiaxin confirms the size of the sealing groove and the specifications of the rubber ring in the waterproof shell project to avoid mismatch between the rubber ring and the groove type purchased by the customer. A groove depth tolerance on the drawing often determines the waterproof performance of the entire batch of products.

If leakage has already occurred on site, first measure the groove depth and rubber ring cross-section, and then check the tightening sequence. The cause can usually be found without changing the mold.

Back to list

Need a housing built for your camera?

Send us your drawings or samples — our engineering team will respond with a feasibility plan and quotation.