Standards and interpretation of shell salt spray test

The test conditions must be written clearly

It is also called salt spray test, and the conclusions cannot be compared under different conditions. Neutral salt spray commonly uses 5% sodium chloride solution. The temperature in the box is controlled at around 35 degrees Celsius. The pH and sedimentation amount of the collection liquid have range requirements. The angle at which the sample is placed affects the residence time of the surface liquid film.

Copper-accelerated acetic salt spray is more acidic and has a fast corrosion rate, making it suitable for rapid screening of decorative coatings; the cyclic salt spray switches between salt spray, wet and dry, closer to the real outdoors. If the report does not clearly state the solution, temperature, angle and duration, the data will have no horizontal reference value.

What to look for in the interpretation

There is more than one level number to interpret. Blistering is graded by area and density, rust is described by number of points and distribution; scratched samples depend on the unilateral corrosion width, that is, the distance spread from the scratched edge to both sides. This indicator can best distinguish the protective ability of the coating system. The photos should include the whole and parts, and mark the sampling location to facilitate comparison between different batches.

For sample parts with assembly relationships, it is also necessary to check whether the threads and sealing surfaces are affected by the accumulation of corrosion products, and whether the adhesion is reduced after the test. Only recording the appearance grade will easily miss the functional degradation.

Specimen preparation also affects conclusions. Cutting and sampling will damage the edges of the coating. Unless the project clearly requires it, complete parts should be taken or submitted for testing in the actual assembly state; oil stains and burrs on the surface should be cleaned before testing, but solvents that will change the state of the coating cannot be used.

Three types of common misjudgments

The first is improper cleaning before the test, and finger grease or processing residual liquid remains on the surface, causing local premature corrosion; the second is that the scratching tool is not consistent with the strength, the scratch depth is different, and the corrosion expansion results are naturally different; the third is that the test is left without cleaning after the test, the salt continues to act, and the reading is severe. What the three have in common is that the test itself deviates from a unified caliber.

  • The report states the solution, temperature, pH, angle and duration.
  • Blistering, rusting, and corrosion expansion are recorded separately, not just given grades.
  • The results will be comparable only if the scratching tool and intensity are consistent.
  • After the test, clean and dry according to regulations, and interpret within a limited time.

The standard practice is to clean and dry according to regulations after the test, complete the interpretation within the agreed time, and keep the photos. The original conditions and photos are attached to the report so that there will be a basis for comparison when changing suppliers later. Weijiaxin records salt spray data and process parameters correspondingly in the surface treatment process, so that the same coating system can be mutually confirmed between different projects.

Back to list

Need a housing built for your camera?

Send us your drawings or samples — our engineering team will respond with a feasibility plan and quotation.