Drawing verification before mold making
The 3D drawings provided by customers often only show the external shape and interfaces, lacking draft angles, wall thickness transitions, and rounded corners. Before mold making, these details must be completed: The main wall thickness is set at approximately 2.5 mm, with a gradual transition at the junction between thick and thin sections. The draft angle is specified as one degree for the outer surface and one and a half degrees for the inner cavity. Areas with insufficient draft will be scratched during trial molding, and there is usually only one opportunity for polishing and repair.
The parting line position, the allowable area for ejector pin marks, and the gate position are also confirmed simultaneously. The parting line is least noticeable when placed on the edge of the visible surface, the gate is positioned away from the decorative surface, and the ejector pin marks fall on the internal ribs or in areas outside the sealing surface.
Mold Structure and Steel Selection
Mass production molds are generally made with one or two cavities. Hot-work die steel is used for the movable and fixed molds, and core inserts are replaced individually based on vulnerable areas. The cooling water channels run along the contour of the cavity, with the spacing controlled at around 30 mm. When the mold temperature is uniform, the shrinkage of the castings is consistent, and the flash is also thin.
The ejection mechanism is arranged according to the shape of the product, and the deep cavity parts are fitted with ejector pin sleeves to avoid white marks. The positions of the slide and the angle pin should be confirmed with the customer, as slide marks will remain on the side of the housing, and it is not advisable to place slides near the waterproof structure.
Mold trial and first article inspection
Mold trials are conducted in two rounds. The first round focuses on filling and demolding, with an emphasis on recording instances of material shortages, scratches, deformations, and the locations of air voids.In the second round, the mold is re-injected according to the adjusted parameters. The first part is taken for full-scale measurement and compared with the drawing item by item. At the same time, the sealing surface is sectioned to inspect the internal quality. Out-of-tolerance items are divided into two categories: those that can be directly corrected by the mold, and those that require changes to the product structure. The latter must be returned to the customer for confirmation.
The process window during mold trialing must be fully recorded, including melt temperature, mold temperature, injection speed, and holding time. The same defect may be caused by multiple parameters. If only the results are recorded and the parameters are not recorded, the second round of adjustments will become trial and error. The window data also serves as the starting point for subsequent mass production settings.
- The mold trial report includes molding parameters, actual measured dimensions, and photographs of the appearance;
- The first part is retained as a sample to serve as a reference for comparison in subsequent mass production.
- A list of items requiring mold modifications should be prepared, indicating the responsible party and the timeline;
- Only after the small-batch trial production has been approved will the production be transferred to mass production scheduling.
Weijiaxin has its own mold workshop, where drawing reviews and mold trials are completed on the same premises. There is no need for inter-factory coordination for mold modifications, making the pace easier to control. By clarifying the structure during the mold development stage, there will be fewer rounds of rework during the mass production stage.