Wall thickness is subject to filling and shrinkage first
Common wall thicknesses for die-cast aluminum housings are between 2.0–3.0 mm. If it is thinner than this, the molten metal cools too fast in the long process, which is prone to cold isolation and insufficient pouring; if it is thicker than this, the thick-walled area cools slowly, making feeding difficult, and internal shrinkage holes and surface depressions increase. Uniform wall thickness is more important than the value itself: adjacent areas have very different thicknesses, cooling rates are different, shrinkage stresses are concentrated, and deformations and cracks often appear at transitions. The wall thickness is also constrained by the thread depth. The effective engagement depth of the M4 thread is about 6 mm. If the wall thickness is too thin locally, it will lead to chipping of the tapping.
The transition should be slow. Add fillets or slope transitions at the steps to avoid sudden changes in right angles; the fillet radius should not be less than one-third of the wall thickness so that the transition area will not become a hot spot. If necessary, hollow out the thick areas and use ribs to maintain stiffness, so that the entire part is close to the same wall thickness.
Strength does not depend on blindly thickening
The shell bears the installation load, wind load and occasional collisions. Most failures are manifested as local dents or screw seat cracks, rather than insufficient overall strength. The wall thickness increased from 3 mm to 4 mm, and the weight and material increased by 30%, but the stiffness improvement was limited; instead, reinforcement ribs were arranged in the direction of stress, the rounded corners at the root of the screw column were increased, and the mounting ears were integrated with the main body, which resulted in a more direct effect. The failure of thin-walled parts is mostly due to overall deformation. When judging, it is necessary to distinguish whether the stiffness is insufficient or the installation surface is uneven.
The layout of the ribs should be particular: the thickness of the ribs should be 0.6-0.8 times the thickness of the main wall. If it is too thick, hot spots will be formed at the root of the ribs; the distance between the ribs should not be too close, otherwise the exhaust and filling of the mold will be poor; the direction of the ribs should follow the flow direction of the molten metal to avoid the formation of dead corners.
How to calculate the cost account
The cost of increased wall thickness is not limited to materials. Extended cycle time, increased mold thermal load, and increased risk of deformation will all push up the cost of a single piece; blind thinning requires higher mold accuracy and injection parameters, and an increase in the scrap rate is also a cost. A reasonable approach is to first determine the wall thickness according to functional partitions: ensure sufficient thickness for the sealing surface and screw columns, thin the large areas of the appearance, and reinforce the non-stressed areas with ribs. Doing a weighing and wall thickness test during the proofing stage can detect the risk of overweight in advance.
- The main wall thickness should be about 2.5 mm, finely adjusted according to the size of the part;
- The rib thickness should be 0.6–0.8 times the main wall thickness, and the root should be rounded;
- The outer diameter of the screw column should be approximately 2 times the nominal diameter of the thread, with reinforcing ribs;
- A slope of 1:3 or above should be made at the transition between thickness and thickness to avoid stress concentration.
Weijiaxin will provide wall thickness distribution and mold plans at the same time during the structural review, allowing customers to clearly see the trade-offs between weight, cost and strength before opening the mold. If the customer has an upper limit on weight, the plan must also leave allowance for coating and fasteners. If the wall thickness is set reasonably, there will be less mold modifications and less rework later.