Material selection of camera housing sealing ring

Look at the working temperature and medium first

Nitrile rubber has good oil resistance and low cost. It is the choice of many indoor models. However, its ozone resistance and weather resistance are average, and it is easy to crack when exposed to the sun for a long time. EPDM has better weather resistance, ozone resistance, and water vapor resistance, and is suitable for long-term outdoor exposure; silicone has a wide temperature range and good low-temperature elasticity, but is weak in oil resistance and tear resistance.

The order of material selection should be to first determine the temperature range and contact medium, and then look at the cost. If there are grease, detergent or asphalt volatiles near the shell, the advantages of nitrile will be established; if there is only rain and ultraviolet rays, EPDM is more reliable. Even if the brand is the same but the formula is different, the weather resistance performance may be quite different. Asking for the material description is more reliable than looking at the color.

Compression permanent deformation deserves more attention than hardness

Hardness only indicates the initial softness and hardness. Long-term rebound depends on compression permanent deformation. The rubber ring is always in a compressed state after installation. If the material deforms irrecoverably at this temperature, the seal will fail after several disassemblies and installations. When selecting materials, you should ask for the hardness and deformation data at this temperature, rather than just looking at the tensile strength.

In terms of hardness, 40–60 Shore A is commonly used for shell seals. If it is too soft, it will easily be squeezed out of the groove; if it is too hard, it will have poor ability to fit uneven surfaces. When there are slight fluctuations in the sealing surface of die castings, medium hardness with sufficient compression is usually more reliable than high hardness.

Several details that are easily overlooked

The same brand of rubber has different molding methods, and the lifespan is quite different. The molded integrated ring has no joints and is more reliable than the bonded ring; the bonded joint is prone to cracking under temperature cycles, and the cracks often appear on the inside first and cannot be seen during assembly.

  • A thin coating of silicone grease before assembly can reduce distortion, but the grease cannot be in long-term contact with EPDM;
  • The rubber ring has a storage period, and its elasticity will decrease after long-term storage, so it is not suitable to be stacked in the same batch with metal parts for a long time;
  • The notch needs to be rounded and deburred, as sharp edges will cut the rubber ring during assembly;
  • It is recommended to replace the rubber ring with a new one after disassembly and maintenance, and do not reuse the old ring that has been shaped.

After the material is selected, the whole machine needs to be verified. Put the assembled prototype into the high and low temperature cycle box, and conduct an air tightness test in the high temperature section and the low temperature section, which can expose the lack of rebound better than a single-point test at normal temperature. Weijiaxin will provide the rubber ring specifications and groove dimensions together during the sampling stage to facilitate customers to match them when purchasing locally. If the old ring is used when the whole machine is repaired, the compression capacity will have been lost, which means the risk of water leakage will be left to the customer.

Back to list

Need a housing built for your camera?

Send us your drawings or samples — our engineering team will respond with a feasibility plan and quotation.