Failure starts from the surface of the cavity
The life of the die-casting mold does not end suddenly, and there are traces of failure. The most common starting point is thermal fatigue cracks on the surface of the mold cavity: the molten metal is repeatedly washed away, and the release agent quickly cools the surface layer, forming fine network cracks, which are initially only near the gate and gradually extend to the molding surface. Once the cracks form a network, the surface of the extruded parts will have raised lines, which cannot be suppressed by polishing.
The second category is erosion and mold sticking. The position directly opposite the gate is washed away by the liquid flow, and the cavity is partially sunken, causing the size to drift; the demoulding slope is insufficient or the surface is rough with aluminum sticking to it. Each mold must be cleaned manually. The clearer it is, the more damage it will cause. The third category belongs to structural problems: slider guide rail wear, ejector pin hole roughening, cooling water channel scaling, manifested as sluggish movement and uneven mold temperature.
Maintenance is based on cycles rather than feelings
Modules are the only objective benchmark for maintenance. Each set of molds is archived to record the cumulative number of molds, last maintenance content and actual measured dimensions of the mold cavity. Routine maintenance is based on fixed mold disassembly and inspection: cleaning the cavity and exhaust groove, checking the ejector pin and slider, and measuring key dimensions. The exhaust groove is blocked by aluminum chips and sludge, and the air cannot be discharged. Undercasting and pores appear subsequently. This cleaning is more valuable than heavy polishing.
Restorative maintenance is often overlooked. The internal stress of mold steel accumulates after repeated thermal cycles. Stress relief and tempering based on the accumulated mold times can postpone the occurrence of cracks. When the cavity is worn to the lower limit of size, repair welding can be performed, but the difference in hardness between the repair welding area and the base metal will become a new starting point for cracks. After repair, it needs to be re-polished and stress relieved.
How to judge when the service life is over
The criteria for mold replacement must be determined in advance, and the decision cannot be made until qualified parts cannot be produced. Three limits are more practical: the key dimensions of the mold cavity exceed two-thirds of the product tolerance, the flash needs to be suppressed by increasing the clamping force, and the cracks are so deep that they cannot be eliminated by polishing. If any one of them is reached, the backup mode switching process will be entered.
- Build a maintenance ledger based on each mold, and the exhaust groove cleaning cycle is shorter than the cavity polishing cycle;
- The cooling water channel is cleaned every quarter, and the temperature difference between the inlet and outlet water is recorded;
- Key dimensions are measured for each maintenance, and the trend is drawn instead of just recording a single value;
- The backup mold is tested and confirmed in advance to avoid starting the main mold when it is stopped.
The mold is the source of the dimensional stability of the housing. Weijiaxin has its own mold workshop, which integrates the mold order ledger and maintenance records into the product files. The first piece after mold change with the same part number is still compared with the original parameters. Customers will not receive goods with different sizes just because a set of molds has been changed.