Parting surface design of die-cast aluminum alloy shell

The position of the parting surface determines the appearance and subsequent work hours

The parting surface is the surface where the movable mold and the fixed mold fit together. The molten metal is finally sealed here during die casting, thus leaving misshaped lines and flash edges. If you choose the wrong location, it will look ugly no matter how you polish it later. The basic principle is to place the parting surface on the non-appearance surface, non-sealing surface, and non-assembly datum surface.

Take the gun shell as an example. The parting surface usually runs along the side edge of the middle part of the shell, avoiding the top surface and the front where the lens window is. If it must fall in a visible area, make the parting line into a decorative groove and use the structure to cover up the traces of craftsmanship, which is more controllable than polishing afterwards. Try to keep the traces in straight lines and avoid folding lines on the plane. It is easy to accumulate flash at the corners of the folding lines, and the edges are also prone to chipping during cleaning.

Allowance for draft and misalignment

The draft angle of the outer wall of aluminum alloy die-casting is generally 1°–2°, and the inner cavity is 1.5°–3°, and the areas with deep cavities and textured surfaces should be increased. If the slope is not enough, the base material will be strained during demoulding, and the stretch marks will still be vaguely visible after powder spraying.

The amount of misformation depends on the fit of the mold guide posts and the distribution of the clamping force. If the cavities on both sides of the parting surface are offset, the wall thickness will be thicker on one side and thinner on the other, and black skin may appear on one side after CNC processing. Weijiaxin measures the amount of mold errors during the mold trial stage, repairs the mold first if it is out of tolerance, and enters the batch without problems. On the same mold, uneven cooling of the fixed mold and the movable mold will also amplify mold errors, and the mold temperature records must be included in the mold trial file.

The relationship between the sealing surface and the machining allowance

If the sealing groove is cast directly, the bottom of the groove will have a demoulding slope and casting roughness, and the compression amount of the apron will fluctuate along the circumference, making the waterproofing unstable. A more reliable approach is to leave a machining allowance of 0.3–0.5 mm on the sealing surface, fine mill it after die casting, and correct the flatness at the same time.

  • The parting surface avoids the plane where the display surface and the sealing groove are located;
  • The appearance surface draft is taken according to the minimum demoulding value to reduce visual deformation;
  • Leave a margin for the plane that needs to be finished, and mark the unified benchmark on the drawing;
  • Use a manual clamp to clean the flash edges, instead of damaging the base material by grinding a large area with a grinding wheel.

Parting surface design is a common agreement between die casting, mold and post-processing. The advantage of having an in-house mold workshop is that the impact on the mold cavity can be assessed on the same day as the drawing is changed. There is no need to transfer information back and forth, and the mold trial cycle is also shortened. If the customer wants to change the structure later, the parting surface is often the first place to be touched. It is more practical to leave room for adjustment during the review.