CNC job skills training to improve processing stability

Training starts with reading drawings and tolerances

The difference in CNC positions is often not whether you can turn on the machine, but whether you can understand the intention of the drawings. If the same position is marked and the datum is wrongly selected, the finished parts will be biased during assembly. This round of training puts drawing interpretation in the first week and requires operators to be able to state the benchmarks, tolerance zones and inspection methods for each critical dimension, rather than just following the procedure.

The key dimensions of the shell are concentrated on the mating surface, sealing groove and screw seat. The training uses real workpieces as teaching materials, allowing operators to find the corresponding position on the three-dimensional coordinate report and understand whether the out-of-tolerance is tool wear, clamping deformation or program compensation failure. Only by pinpointing the cause can we make adjustments.

Clamping and tools are the entrance to stability

Most deformation of thin-walled shells occurs in clamping. If the clamping force is too large, the workpiece will rebound when released and the flatness will be exceeded. During the training, the clamping sequence, support point position and clamping force were standardized, and a dial indicator was used to measure before and after clamping, so that the operator could see the difference himself. There is a unified wear judgment standard for cutting tools. If the wear band on the flank surface exceeds 0.2 mm, it should be replaced.

Cutting parameters are no longer set by individuals based on experience. A recommendation table is given for each material and tool combination. There are intervals for speed, feed and depth of cut. The reasons for exceeding the intervals must be recorded. In this way, when people and shifts are changed, the surface roughness processed will not be significantly layered.

First article self-inspection and exception reporting

The training requires that the first article of each batch be self-inspected and signed by the operator. The self-inspection items are listed in a short list according to the key dimensions and appearance defects of the drawings, without the need for a complete inspection sheet. If an abnormality is found during the self-check, the machine must be shut down first and then reported. It is not allowed to wait for judgment while doing the work. This rule appears to slow down the pace of output, but actually reduces the rework of the entire batch.

  • The first piece self-inspection covers three categories: mating surface size, sealing groove depth and appearance;
  • First piece confirmation must be done again after changing tools, procedures, and materials;
  • Shut down the machine for inspection if the size of three consecutive pieces deviates in the same direction;
  • A practical assessment is conducted every quarter, including fault judgment and parameter adjustment.

The purpose of training is to transfer stability from personal experience to process. Weijiaxin has arranged this work into a regular plan, with mentoring and assessment in parallel. What customers can feel is that the same shell is assembled across batches without picking parts, and there is no need to re-run it when returning the order.

Back to list

Need a housing built for your camera?